Q. When variations are noticed in the front surface reflection, the test piece should beinspected for possible near surface discontinuities by: (Solved)

1. Using a lower frequency transducer

2. Using a higher pulse energy

3. Inspecting from the opposite side

4. Calibrating on a smaller diameter flat bottom hole

  • c. Inspecting from the opposite side